The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
This study focuses on the influence of loading MWCNTs in In2O3-based DSSCs. In2O3-MWCNTs were prepared by sol-gel method via spin coating technique and annealed at 450 °C. The structural, morphology, and electrical properties of the photoanodes were characterized by means of XRD, AFM and FESEM, and J-V curve measurement and EIS properties, respectively. Incorporation of MWCNTs in In2O3 improved the...
Indium oxide-multi-walled carbon nanotubes (In2O3-MWCNTs) were prepared by sol-gel method for DSSCs. The synthesis of indium oxide (In2O3) was carried out by dissolving indium chloride (InCl3) in a solvent of 2-methoxyethanol. Different annealing temperatures of 400, 450, 500, 550, and 600 °C were proposed in this study. The changes in the structural properties were analyzed by means of X-ray diffraction...
ZnO thin films were deposited by Rf Magnetron sputtering on glass substrates at various deposition temperature in the range of 100–400°C. The thin films characterized using field emission scanning electron microscopy (FESEM), atomic force microscopy (AFM) and UV-VIS-NIR spectrophotometer for morphology and optical properties study. All the films are transparent in the visible region (400–800 nm) with...
Samples of La0.67Sr0.33Mn1−xTixO3 with concentration of x = 0.00, 0.20, 0.40 and 0.60 were prepared using the sol gel method, deposited on quartz and ITO substrate by using a spin coater. The samples were calcined at 500°C for an hour. From the Scanning Electron Microscope (SEM) micrograph, it showed that the particles size increased as the concentration of doping was increased. Each sample showed...