The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Polyurethane (PU) flexible foams were synthesized by substituting a portion of base polyether polyol with soybean oil-derived polyol (SBOP) as well as well-known substituent: crosslinker polyol and styrene acrylonitrile (SAN) copolymer-filled polyol. Increases in compression modulus were observed in all substituted foams and the most substantial increase was found in the 30% SBOP-substituted sample...
The efficiency of two compatibilization methods, adding premade copolymers versus in situ formation of copolymers, were compared by evaluating the minor phase size and size distribution. Premade diblock copolymers were formed by coupling amine terminal polystyrene (PS-NH 2 ) with anhydride terminal poly(methyl methacrylate) (PMMA-An) in solution. Mid-functional PMMA was coupled with the PS-NH...
Coupling functionalized polymers at the interface between them is a major route to compatibilize immiscible polymer blends. The reactively formed block or graft copolymers both stabilize morphology and enhance adhesion. Reactive coupling can also be used to increase the adhesion between coextruded films and for solvent-free synthesis of block copolymers, producing new nanostructured materials, not...
The effect of block copolymers on the cocontinuous morphology of 50/50 (w/w) polystyrene (PS)/high density polyethylene (HDPE) blends was investigated using symmetric polystyrene–polyethylene block copolymers (PS–PE) with molecular weights varying from 6 to 200kg/mol. The coarsening rate during annealing was compared to the Doi–Ohta theory. An intermediate molecular weight PS–PE, 40kg/mol, showed...
Phthalic anhydride terminated polystyrene (PS-An) and styrene-maleic anhydride copolymer (SMA) were compared as a compatibilizer at low loadings (<10wt%) in 70/30 polyamide 66 (PA66)/polystyrene (PS) blends. Compatibilization efficiency was judged by morphology of the blends and the extent of interfacial coupling to copolymer. Fluorescent labels of functional PS's (anthracene and pyrene for PS-An...
We have visualized a fluorescently-labeled poly(styrene-b-methylmethacrylate) (NBD-PS-b-PMMA) block copolymer on the surface of a polymethylmethacrylate (PMMA) drop in a polystyrene (PS) matrix. Confocal microscopy revealed that the block copolymer distributed uniformly on the drop surface before deformation. However, in shear flow the copolymer concentration was higher at the tips and edges of the...