The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Lithium manganate spinels with the formula Li1+xMn2−xO4 undergo lithium↔proton ion exchange to form a protonated λ-MnO2-type phase. The Li1+xMn2−xO4 phases are metastable, and preparation at temperatures in excess of 400 °C results in phase separation. By partially substituting the manganese with cobalt, single-phase spinels of formula Li1.33−x/3CoxMn1.67−2x/3O4 (0<x<1) can be prepared with...