The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
(BaTiO_3)_{0.84}(CeO_2)_{0.16} thin films were prepared by electron beam evaporation method. X-ray diffraction and scanning electron microscopy revealed the amorphous structure for the as-prepared films. The thin films were annealed at temperatures: 200, 300, 400 and 500C for 1 h in air. Small and low intensity crystalline peaks were observed at annealing temperature of 200C for 1 h. The intensity...
Cadmium selenide thin films with different pH values (pH = 10, 11, 12 and 13) are produced on glass substrates at 50°C for 3 h by chemical bath deposition technique. The structural, morphological and optical properties of the films are characterized by X-ray diffraction, scanning electron microscopy and optical absorption spectroscopy, respectively. The obtained films have hexagonal structure. The...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.