The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
A newly designed TiAl alloy containing W, Nb, and B was produced through magnetic-flotation-melting method. Mass production of this TiAl-based alloy, 15 kg ingot size, which is quite different from the 0.05 kg small ingot produced by arc-melting, has a large effect on the metallurgical properties, such as the grain size and the phase structures of the alloy. Heat treatments were carefully designed...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.