The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Samples of cathode material were synthesized from a highly dispersed precursor containing 0.002 at.% Sr. The synthesis was performed from a mixture of the precursor with some overstoichiometric excess of LiOH at 720 °C in oxygen atmosphere. Part of the samples were coated with a thin film of Li-borate glass. The cathode active material (CAM) was mixed with 15 wt.% of Teflonized acethylene black and...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.