The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Monolithic alumina and alumina–silver composite containing 15.0vol.% of silver have been fabricated via pressureless sintering approach. By virtue of the inherent high vapour pressure of silver at elevated temperature during sintering, a decreasing silver gradient was observed between the bulk and the surface of the composite material. As a consequence of this phenomenon, a functionally graded structure...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.