The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Thin film produced by exploding wires is affected by many factors; one of such factors is the energy depositing rate. The research in this paper focused on measuring the voltage and current of an exploding copper wire that was 15 cm long and 0.3 mm in diameter. The time-dependent wire resistance and the energy deposited into the wire were deduced from the measured voltage and current, and the maximum...
Thin film production by exploding wires is affected by many factors; one of such factors is the energy deposition rate. The research in this study focused on measuring the voltage and current of an exploding copper wire that was 15 cm long and 0.3 mm in diameter. The time-dependent wire resistance and the energy deposited into the wire were deduced from the measured voltage and current, and the maximum...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.