The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
The 0‐3 type CaBi4Ti4O15:30 wt%BiFeO3 composite shows much better high‐temperature piezoelectric properties than the single‐phase CaBi4Ti4O15 or BiFeO3 ceramics. The composite with 0‐3 type connectivity exhibits a high density of 7.01 g/cm3, a saturated polarization of 21.5 μC/cm2 and an enhanced piezoelectric d33 of 25 pC/N. After the poled composite was annealed at 600°C, its d33 is 21 pC/N at room...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.