The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
BaTiO3 (BT) ceramics with fine grains were sintered at an ultra low temperature of 180°C by means of a novel sintering method named as cold sintering (CS). For CS, the hydrothermal precursor solutions were incorporated into the ceramic powders, and pressure was also applied during sintering. After annealing at 900°C, the obtained samples exhibit dense microstructures and relative densities higher...
Pb 0.94 La 0.06 Nb 2 O 6 ceramics were prepared by solid state reaction of high energy ball milled precursor powders. Calcination temperature of the milled precursor was lowered to 850°C. Single orthorhombic phase was obtained after the ceramics were sintered at 1205°C and 1230°C. Lattice parameters, porosity and grain size were all affected by sintering temperature...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.