The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Low-temperature roasting, selective decomposition and water-leaching were used to extract nickel and copper from low-grade nickel sulfide ore with highly alkaline gangue. The effects of variable factors, such as the dosage of roasting additives, the ore particle size, roasting time and roasting temperature, selective decomposition temperature and leaching temperature on the conversion of metals were...
Due to stringent environmental requirements and the complex occurrence of valuable metals, traditional pyrometallurgical methods are unsuitable for treating low-grade nickel-copper matte. A clean and sustainable two-stage sulfating roasting and water-leaching process was used to simultaneously extract valuable metals from low-grade nickel-copper matte. Ammonium and sodium sulfate were used as sulfating...
This paper investigated the electrolytic production of Ti5Si3/TiC composites from TiO2/SiO2/C in molten CaCl2. The solid-oxide oxygen-ion-conducting membrane tube filled with carbon-saturated liquid tin was served as the anode, and the pressed spherical TiO2/SiO2/C pellet was used as the cathode. The electrochemical reduction process was carried out at 1273 K and 3.8 V. The characteristics of the...
In this work, a two-stage sulphuric acid roasting and water leaching system was chosen to extract valuable metals from Chinese low-grade nickel sulphide ore. By optimizing the two-stage roasting process, first roasting temperature at 295°C with particle size of 80–91 μm with an acid-ore ratio of 1.1:1 for 2 h, and second roasting temperature at 620°C for 2 h, it was found that more than 98% of the...