The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Tensile properties and fracture behavior of X80 pipeline steel exposed to corrosion environments with different H2S/CO2 partial pressure ratios were investigated through slow strain rate tests (SSRT). The results show that the tensile properties of X80 steel were damaged in H2S/CO2 environments. The tensile strength and elongation to failure of X80 steel decreased significantly with increasing H2S/CO...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.