The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Amorphous wires of CuZrAl and CoFeSiB alloys were fabricated by in-rotating-water melt quenching (IMQ) and glass coated Taylor (GCT) techniques, and the diameters of the amorphous wires prepared by the IMQ are in the range of about 50 to 200 mum, while by the GCT are in the range f about 5 to 18 mum. The stress-strain curves of the Cu50Zr46Al4 amorphous wire show a nonlinear deformation after the...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.