The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Five percent of Fe-doped ZnO (ZnO:Fe) thin films were deposited on Pt/TiO2/SiO2/Si substrates by a spin-coating method. The films were annealed without (ZnO:Fe-0T) and with a pulsed magnetic field of 4 T (ZnO:Fe-4TP) to investigate the magnetic annealing effect on the resistance switching (RS) behavior of the Pt/ZnO:Fe/Pt structures. Compared with the ZnO:Fe-0T film, the ZnO:Fe-4TP film showed improved...
The ionic liquids containing Cd and Zn, which served as the metal-chalcogenides precursors, were synthesized and reacted with Na2S to synthesize the ionic-liquid-capped semiconductors. The products were detected by XRD and TEM. The results demonstrated that the CdS was composed of 5–6 nm monodispersed nanocrystals. At the same time, the ZnO composed of 1 μm hexagonal-disk nanostructure was prepared...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.