The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
CuSn10 pre-alloyed bronze with iron and graphite powders were mixed, pressed and sintered for the bronze pad fabrication. The powder mix was pressed under pressure in the range of 100-600 MPa and sintered at temperatures between 780-850°C. The optimum compression was at 500 MPa and the optimal sintering temperatures was 730°C. 2 wt.% of graphite addition was sufficient to adjust the friction and wear...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.