The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
The silicon-doped BiVO 4 film was fabricated by modified metalorganic decomposition (MOD) method. XRD analysis indicated that the crystal size of the BiVO 4 film was decreased from 32.4nm to 23.9nm by doping Si. The measurements of FT-IR spectra and the water contact angle showed that doping Si could elevate the surface hydrophilicity of the BiVO 4 film. The phenol elimination...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.