The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
In this study, we measured spin polarization of electrons field-emitted from a topological antiferromagnetic Cr(001) surface, which is expected to generate a high and stable spin-polarized electron beam. When the Cr thin film deposited on a W<001> tip was thicker than 20 nm, the spin polarization of the field-emitted electrons reached 50%. Furthermore, the magnitude and direction of the spin...
We observed the Verwey transition, metal-insulator transition, in a spin-polarization of field-emitted electrons from a topmost surface of a <110>-oriented magnetite whisker by means of field-emitted electrons polarimetry. The measurements of spin polarization of field-emitted electrons from a magnetite whisker were carried out ranging from 40 to 300 K of tip temperature under UHV condition...
We measured temperature dependence of a spin polarization of field-emitted electrons from a single-crystalline magnetite (Fe 3 O 4 ) whisker with 〈110〉 orientation. The spin polarization of emitted electrons began to increase above 130K corresponding to the temperature of Verwey point (T v ). The increase is considered as reflection of the change of the spin state near the...
We measured spin polarization of electrons field-emitted from half-metallic Co 2 MnSi thin film grown on a W(001) facet via chromium buffer layer using Mott scattering. For spontaneously magnetized samples, values of polarization at room temperature were observed in a range from 10% to 46% and the polarization direction was 〈110〉 orientation of substrate tungsten, which agreed with an easy...