The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
We demonstrate passive mode-locking of a Nd:Sc0.2Y0.8SiO5 laser using a semiconductor saturable absorber mirror. The pulse train shows output power of 0.5 W and pulse duration of 3.5 ps at repetition rate of 118 MHz.
Recently, diode-pumped solid-state lasers based on disordered Nd-doped crystals have attracted significant attention. In mode-locked operation they have a potential to generate tunable laser radiation with pulse duration in sub-picosecond time scale as well as to emit muti-wavelength ultrashort pulses which makes them attractive as a source for terahertz generation [1]. Nowadays, the binary and ternary...
An experimental investigation on the laser performance of an α-oriented Tm,Ho: YAIO3 crystal end-pumped by a wavelength tunable Ti:Sapphire laser is presented in this paper. Single- and dual-wavelength operations of Tm,Ho:YAIO3 lasers have been investigated in detail. Maximum output powers of 890mW at 2119nm, 836mW at 2103nm and 487mW at 2130nm for the α-oriented Tm,Ho:YAIO3 crystal have been obtained,...
Effective diode-pumped cw tunable laser action of a new crystal Yb3+:Lu2Si2O7 (LPS) is demonstrated for the first time to our knowledge. The advantage of Yb: LPS is the presence of effective low-symmetry monoclinic structure and its single crystallographic site, which are benefit for the low threshold and high output energy. With a 5-at% Yb: LPS sample, we achieved 2.22 W output power at 1070 nm....
Diode-pumped stable CW mode-locked laser in Yb:LuAG crystal was demonstrated. The pulse duration of 7.63 ps was achieved without any negative dispersion elements. With pump of 8 W, output power was 610 mW with repetition rate of 86 MHz.
Using a novel broadband Yb-doped crystal close-loop cooled at -130degC we demonstrate a 2-6-W multi-kilohertz amplifier delivering sub-200-fs pulses with energies up to 2 mJ. This technology is straightforwardly scalable toward a kHz-repetition-rate multi-mJ output.
Absorption, photoluminescence spectra and CW lasing parameters of an Yb3+- and Na+-codoped CaF2 laser crystal are measured in the temperature range from 5 K to 290 K. The crystal appears to be a promising host for broadband multi-mJ kHz CW-pumped regenerative amplification.
A diode pumped cw laser operation based on 5-at.% doped Yb:GSO crystal was reported. The optical conversion efficiency of 64.5% at 1089 nm was achieved and the tuning range extends to ~65 nm.