The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
The polarization behaviour of a mild steel has been studied on static and rotating electrodes in solutions containing various concentrations of CO 2 , HCO -3 and CO 2-3 , from which it is shown that the lower bound of the intergranular stress corrosion cracking domain occurs at potentials a little above those at which a first oxidation peak is observed. The...
The potentials at which intergranular stress corrosion cracking occurs in a mild steel exposed to solutions of various pH values, obtained by varying the concentrations of CO 2 , HCO -3 and CO 2-3 have been determined, as have those potentials at which quasi-cleavage occurs in similar but lower pH solutions. The potential range for intergranular cracking is...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.