The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
The effect of treatment in weld surface on four-point bend fatigue properties and fracture characteristic of Ti–6.5Al–2Zr–1Mo–1V alloy by vacuum electron beam welding were tested and analyzed. When the excess weld metal and excess penetration are removed, the high fatigue strength of joints can be obtained. When the excess weld metal and excess penetration were not removed, the fatigue strength of...
A nanostructured layer was fabricated by using fast multiple rotation rolling (FMRR) on the surface of Ti-6Al-4V alloy, with grain size 10–19 nm in the top surface layer by means of XRD and TEM analysis. A deformation layer with thickness about 80 μm is clearly observed in the cross section of FMRR sample. The microhardness of the FMRR sample has an obvious change along the depth from about 368 HV...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.