The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
ZnO micro-structures were deposited by aqueous chemical growth on Si (100) substrates, their morphology and size depending on the growth period. Characterization of the structures was performed using X-ray diffraction, scanning electron microscopy and Raman spectroscopy. Photoluminescence spectra recorded at 18 and 295K for 325nm CW excitation indicated that these are strongly affected by the morphology...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.