The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Low carbon steels have been joined using an infrared processing technique with copper as the filler material. Single lap specimens were prepared. The joining temperatures were 1100 °C, 1125 °C, and 1150 °C with joining time ranging from 0 to 2 minutes in flowing argon. Excellent wetting between the base materials and the filler was observed for all samples. The joint shear strength was determined...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.