The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Chiral polymer P-1 incorporating (R,R)-salen-type unit was synthesized by the polymerization of (R,R)-1,2-diaminocyclohexane with 2,5-dibutoxy-1,4-di(5-tert-butylsalicyclaldehyde)-phenylene (M-1) via nucleophilic addition–elimination reaction, and chiral polymer P-2 incorporating (R,R)-salan-type unit could be obtained by the reduction reaction of P-1 with NaBH 4 . The fluorescence response...
The chiral polymer was synthesized by the polymerization of 4,7-diethynylbenzo[2,1,3]-thiadiazole (M-1) with (R)-6,6′-dibutyl-3,3′-diiodo-2,2′-bis(diethylaminoethoxy)-1,1′-binaphthyl (R-M-1) via Pd-catalyzed Sonogashira reaction. The chiral polymer has orange fluorescence due to the extended π-electronic structure between binaphthyl unit and benzo[2,1,3]thiadiazole (BT) group via ethynyl bridge. The...
The chiral polymer P-1 was synthesized by the polymerization of (R)-6,6′-dibutyl-3,3′-diiodo-2,2′-bisoctoxy-1,1′-binaphthyl (R-M-1) with 5,5′-divinyl-2,2′-bipyridine (M-1) via Pd-catalyzed Heck reaction. P-2 and P-2′ were prepared by Wittig–Horner reaction of (R)-6,6′-dibutyl-2,2′-bisoctoxy-1,1′-binaphthyl-3,3′-dicarbaldehyde (R-M-2) with 5,5′-bis (diethylphosphonomethyl)-2,2′-bipyridine (M-2) in...
A unique crystallization behavior of poly(l-lactide) (PLLA)/poly(d-lactide) (PDLA) stereocomplex was observed when a PLLA/PDLA blend (50/50) was subjected to specific melting conditions. PLLA and PDLA were synthesized by ring opening polymerization of l- or d-lactide using zinc lactate as catalyst. PLLA/PDLA blend was prepared through solution mixing followed by vacuum drying. The blend was melted...
Regular polysulfone (PSF) honeycomb film with micron-sized cells was prepared by casting the solution in an atmosphere with high humidity. Water droplets acted as the template around which the PSF in the solution assemble. In this paper, the effects of atmosphere humidity, solution concentration, and the PSF molecular weight on pore size were discussed; the influence of storage time of casting solution...