The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
The evolution of weld displacement, or the thickness of welding stack, with welding time during resistance welding of thermoplastic composites was characterised, and based on this the possibility of using displacement data for process monitoring and processing window definition was investigated. Resistance welding of glass fabric reinforced polyetherimide using a metal mesh as the heating element...
The strength and failure modes of resistance welded thermoplastic composites were investigated. Special attention was paid to the effect of basic characteristics of the adherends such as fibre–matrix adhesion and fibre orientation. 8HS woven GF/PEI composites were resistance welded. Intralaminar failure was found to be the major failure mechanism for the well welded joints, consisting of either fibre–matrix...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.