The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
BiFeO3-based composite films were fabricated onto the Pt/Ti/SiO2/Si(100) substrates by a chemical solution deposition (CSD) method using the precursor solutions with various excess iron composition followed by annealing at 923 K for 30 minutes under oxygen gas flow. Coexistence of spontaneous magnetization and remanent polarization could be obtained in the BiFeO2-based composite films with high excess...
FeOx-BiFeO3 composite films were fabricated by a chemical solution deposition (CSD) method onto the Pt/Ti/SiO2/Si(100) substrates. The remanence magnetization of almost 2 emu/cm3 and the magnetic coercive field of 1.5 kOe was obtained due to the formation of the magnetic oxide phase at the composition of Fe/Bi=1.25 with the annealing temperature of 923 K for 30 min under the oxygen flow. In this specimen,...
Set the date range to filter the displayed results. You can set a starting date, ending date or both. You can enter the dates manually or choose them from the calendar.